Hi Mohanraj,

Normally potable water is/ may be used/allowed for hydrotest for CS (SA 106 Grades) and LAS material like P11, P22, etc. However please check with client and their specific requirement for quality of water.

Thanks,
Warm Regards,

Rajnish Dixit
Lead - QA-QC/QMS/Welding/NDT/Inspection
+91 972 4200 357

On Fri, May 11, 2018 at 10:06, Mohan
<ggnanamalli@gmail.com> wrote:
Dear Experts,

We are installing HRSG (Heat Recovery Steam Generator) consist of Alloy Steel (P11, P22) and Carbon steel SA106 Gr.B tube bundles.

 In our past experience we did hydro test with demineralized water (DM) but in current project there is scarcity in procuring of DM water can we proceed with Hydro test with Normal RO water.

IF not water are major consequences to tube bundles.

Regards
G.Mohanraj

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35737] Bend Test and Tensile Test failed for ET45 Micro Welded Coupon

Hi As its %elongation is very low  Better try buttering on jt surrace with ductile consumable like pure Ni i. E Ni1 And later weld jt with c...