Dear all,
Mat CSteel
Code 31.3

I have wps gtaw+smaw 12.7mm qualified by impact as per 31.3
Range is 6.35 to 18.7mm

Can generate separate wps only for GTAW (deposits thk on pqr is 4mm)

6.35  to 14.35(6.35+8mm)??

--