Monday, April 2, 2018

Re: [MW:27610] USE OF WPS

Yes, Electrode Dia is not essential variable

On Sun, Apr 1, 2018 at 8:55 AM, Nachhattar Singh <nachhattar1947@gmail.com> wrote:

Dear Experts

 

I have a WPS and PQR approved for 13% Cr. For 3.2 mm Electrode.

My question is if the same WPS can be used for use of 4.0 mm electrode.

 

If yes, then please give reference of the code / standard.

 

Kind regards  

 

N. S. Gurm

 

PLEASE THINK BEFORE PRINTING

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...