Re: [MW:27403] Re: If a welder is qualified with SS (Stainless Steel) GTAW, He can weld CS Carbon steel GTAW?

Hi, 
Cannot weld refer asme sec-9 ed.2017, table qw-356, backing gas deletion is essential, and refer qw-351 to confirm.

Regards, 
Bala. R

On 28 Feb 2018 1:43 pm, "chandrakant mohikar" <crmohikar@gmail.com> wrote:
Coceptually, though he is eligible, he has to be qualified / PQR etc for specific welding WPS etc. 

Chandrakant Mohikar
(Ex. PDO CSR (Head - HSSE & QA)

On 28 Feb 2018 11:39 a.m., "Welding and material" <koswaraabi@gmail.com> wrote:
if we talked about F no on the ASME IX F no associated to A no
for P no and F no SS GTAW Qualified for CS, but we must see para 404.15 then see QW 432 and see Note 1 and then going to QW 433 for A no thanks

Pada Sabtu, 24 Februari 2018 17.03.47 UTC+7, PK menulis:
Dear Sir,

If a welder is qualified with SS (Stainless Steel) GTAW,  He can weld CS Carbon steel GTAW? Need code Referance...

Thanks.
PKM

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...