Re: [MW:27379] If a welder is qualified with SS (Stainless Steel) GTAW, He can weld CS Carbon steel GTAW?



It is omission or deletion


On Sat, Feb 24, 2018 at 5:10 PM, jaffar ali riyas mohamed nizamin <jaffarqc1987@gmail.com> wrote:
Dear Bro,

According to QW 352 : deletion of backing is an essential variable .
QW : 420 Base metal grouping :  welder is qualified for P.no 1 to 15F. But the only thing is Backing gas. 



Regards 
M.Riyas 
+968-97193523

On 24 Feb 2018 2:03 pm, "PK M" <pkmqaqc@gmail.com> wrote:
Dear Sir,

If a welder is qualified with SS (Stainless Steel) GTAW,  He can weld CS Carbon steel GTAW? Need code Referance...

Thanks.
PKM

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...