Saturday, February 24, 2018

Re: [MW:27373] If a welder is qualified with SS (Stainless Steel) GTAW, He can weld CS Carbon steel GTAW?

Please check gas backing is essential variable for welder qualification. 


On Sat, Feb 24, 2018 at 6:23 PM, sankar rao
<sankarkorukonda@gmail.com> wrote:
If welder qualified with SS 
(GTAW Process),
He can weld CS ( GTAW Process)
Because of F.No's same for both SS &CS  for GTAW 
SS ---- F.NO 6.  SFA NO. 5.9
CS----- F.NO 6.   SFA NO. 5.18

On 24 Feb 2018 14:50, "'Prashant Panchal' via Materials & Welding" <materials-welding@googlegroups.com> wrote:
Since he may have used backing gas for SS gtaw he will not be qualified for carbon steel as we do not use backing gas for cs material. 
Alternatively u will have to use backing gas for cs as well


On Sat, Feb 24, 2018 at 3:33 PM, PK M
Dear Sir,

If a welder is qualified with SS (Stainless Steel) GTAW,  He can weld CS Carbon steel GTAW? Need code Referance...

Thanks.
PKM

--
https://materials-welding. blogspot.com/
https://www.linkedin.com/ groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@ googlegroups.com.
Visit this group at https://groups.google.com/ group/materials-welding.
For more options, visit https://groups.google.com/d/ optout.

--
https://materials-welding. blogspot.com/
https://www.linkedin.com/ groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@ googlegroups.com.
Visit this group at https://groups.google.com/ group/materials-welding.
For more options, visit https://groups.google.com/d/ optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...