This practice is considered to be a good engineering practices. BPV codes can't mandate all , many of such things has to come from the fabricators' sound engineering judgement and adopted practices.

 

Please see below the extract from API-RP-582, on the requirements of back purging.

 

P.Goswami.P.Eng, IWE.

Welding & Metallurgical Specialist

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgoswami@quickclic.net,pradip.goswami@gmail.com

M(in India-Till 26 Feb, 2018)- 8336816470

 

7.3 Back purging is required for the GTAW and GMAW processes for welding materials having a nominal chromium content greater than 2-1/4 %, unless the joint is ground or back gouged to sound metal.

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of pradip kumar Sil
Sent: February 21, 2018 3:09 PM
To: materials-welding <materials-welding@googlegroups.com>
Subject: Re: [MW:27361] Cromium limit to maintain back purging

 

Dear everybody,

Can anybody pls give me any code reference regarding this issue. I searched B31.1 , B31.3,  ASME but i did not find  minium chrimium percentage written on the code.

 

Is code silence regarding this issue.

 

Waiting for your valuable reply.

 

thanks in advance

 

regards

pradip

 

On 20 Feb 2018 12:19 pm, "Kannayeram Gnanapandithan" <kgpandithan@gmail.com> wrote:

ref B31.1 or B31.3, and lot of books 

 

Virus-free. www.avast.com


THANKS & BEST REGARDS,

KG.PANDITHAN, BE, IWE,  AWS-CWI, CSWIP 3.1,

CONSULTANT-WELDING & QUALITY

Mobile no: +919940739349

 

On Tue, Feb 20, 2018 at 12:39 PM, pradip kumar Sil <pradipsil@gmail.com> wrote:

Dear Sir,

Can you pls provide me code references.

Thanks in advance

Pradip

 

On 20 Feb 2018 8:53 am, "Kannayeram Gnanapandithan" <kgpandithan@gmail.com> wrote:

Grater than 3% Cr, purging

 

On 20-Feb-2018 9:51 am, "pradip kumar Sil" <pradipsil@gmail.com> wrote:

Dear everybody,

Can anybody inform me minimum how much percentage of cromium limit to maintain back purging with code reference.

Thanks in advance

Pradip

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...