Saturday, February 17, 2018

Re: [MW:27340] Preheating requirements

It is important that when you ask a question of this type you mention what is the Construction Code that you are using or that your client is requesting or maybe you just use an X Code as a reference to justify your work.
I can recommend the Non-Mandatory Appendix R of Section VIII Div. 1 or the PWHT Tables of paragraph UCS-56 of the same Section VIII Div. 1.
Regards!.

2018-02-17 3:59 GMT-06:00 <manojmuthuraj955@gmail.com>:
Dear experts,

We are doing tube to tubesheet welding as follows
Tubesheet thk - 150mm (SA 516 Gr.70)
Tube - 30 X 2.5thk ( SA 179)

If preheating is required for this welding or not? Kindly give your comments with reference code

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.



--

Ing. José Juan Jiménez Alejandro

Soluciones en Soldadura e Inspección

Cel. 812 352 4606

Skype: jjjimeneza

Twitter: @jjjimeneza



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...