Re: [MW:27321] Filler selection

It's better to use  309L

On 06-Feb-2018 6:14 PM, "ramón ignacio briceño" <bricenori@hotmail.com> wrote:
Dear Sir,

Please use a filler welding like 309L to butter CS A105. One pass that cover all area of the CS side. Then complete the process joint  308L material with CS A105 buttering.
This practice facilitate the joint between the austenite phase of the 308L SS and the ferritic phase of the CS  A105.
And you have a welding free of cracking and confidence to service.
Best regard,
Ramon Briceno
Metallurgical Engineer.


From: materials-welding@googlegroups.com <materials-welding@googlegroups.com> on behalf of GALAXY INDUSTRIES PRASHANT PANCHAL <pipanchal@live.com>
Sent: Tuesday, February 6, 2018 2:59:43 AM
To: materials-welding@googlegroups.com
Subject: [MW:27316] Filler selection
 
Dear Experts,

Please suggest me that can we use ER308L filler wire for welding Seamless Pipe A312 TP 304 to Coupling A105 or Please suggest the correct one.

With Best Regards, 


Prashant Panchal 




--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...