Dear sir,

Could someone please advise what should be the fabrication tolerances for piping per B31.3

Per Mr Thomson SA530 the scope doesn't.

 

Best Regards,

Umar

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Thompson, Dennis
Sent: Sunday, January 28, 2018 4:27 PM
To: materials-welding@googlegroups.com
Subject: RE: [MW:27301] Fabrication tolerances

 

Umar,

 

Per the 2015 edition of Section IIA of the ASME BPVC:

 

 

Regards,

D. Thompson, P. E.

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Umar Rashid Makrani
Sent: Sunday, January 28, 2018 7:59 AM
To: materials-welding@googlegroups.com
Subject: [MW:27300] Fabrication tolerances

 

Hi

Could someone please advice on what should be straightness tolerance for piping fabrication being carried out as per ASME B31.3

--

 

With Best Regards,
Umar Rashid Makrani, PMP® ,

 API653, NACE CIP-2, LEEA Registered Engineer.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...