Re: [MW:27309] Re: Weld Repair Procedure as per API 1104

Dear Mr. Madhu,
It is not mandatory. It says if required (2013 edn).

Jayapal 

On Tuesday, 24 November 2015 17:16:26 UTC+8, madhusoodhanan nair wrote:
Dear Members

    As per API1104 Latest edition below mentioned repair procedures is mandatory.

1.Full thickness repair.

2. Cover pass repair
3.Partial  thickness repair
4.Internal Partial thickness repair
5. Back weld reapir

 Note:- Refer Clause 10.3,10.3.1,10.3.2


Regards
Madhusoodhanan  Nair.G




--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...