It depends on the Applicable code. Snap shot of ASME B31.3 given below.

Inline image

Inline image


Refer ASME B31.3, Table 341.3.2 for the type of service

Thanks & Regards

J.Gerald Jayakumar

0091-9344954677



On Thursday, February 1, 2018, 9:55:37 AM GMT+4, 'Sankaran Sp' via Materials & Welding <materials-welding@googlegroups.com> wrote:


Dear Friend,

Thanks for your reply,

My doubt is How much height of weld metal can be allowed as inner penetration?since inner penetration clearly seen in RT film and reported, but end client is asking acceptable limit. Can you give?      

Regards,
Sankaran.SP
Welding & Metallurgy expert
Cell no: 9486409307


On Wednesday 31 January 2018, 5:31:06 PM IST, 'james gerald' via Materials & Welding <materials-welding@googlegroups.com> wrote:


There are lot of Factors involved in Radiography to determine the Density Variation for the ID penetration depth. Moreover you use a Double wall viewing and it is very difficult to determine.

Other methods include

1. Boroscopy
2. Ball run Test. A steel ball with the required diameter shall be passed through the tubes and determine the depth of penetration.

Thanks & Regards

J.Gerald Jayakumar

0091-9344954677



On Wednesday, January 31, 2018, 2:52:31 PM GMT+4, 'Sankaran Sp' via Materials & Welding <materials-welding@googlegroups.com> wrote:


Dear Experts,

During pipe to pipe welding by single V butt joint by GTAW process (example : 1" XXS P91 pipe), there is a weld reinforcement over the groove and maintained 2 to3 mm of height, such a way ID penetration is also there. How much of height ID penetration is allowed? which is to be checked by RT exam. Kindly clarify and give me any supporting/ document  reference.

Regards, 

Sankaran.SP
Welding & Metallurgy expert
Coimbatore, India

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...