Thursday, February 22, 2018

[MW:27364] Re: What is the allowable inner penetration during pipe wedling

Sankaran,

I believe you need also to check on what WPS does state.

On Wednesday, January 31, 2018 at 5:52:34 PM UTC+7, sankaran sp wrote:
Dear Experts,

During pipe to pipe welding by single V butt joint by GTAW process (example : 1" XXS P91 pipe), there is a weld reinforcement over the groove and maintained 2 to3 mm of height, such a way ID penetration is also there. How much of height ID penetration is allowed? which is to be checked by RT exam. Kindly clarify and give me any supporting/ document  reference.

Regards, 

Sankaran.SP
Welding & Metallurgy expert
Coimbatore, India

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...