We are facing confusions in fit-up during equal lateral branches 
fit-up for 12 "× 12" pipe  Drawing  (

As per the formula 
LCB(long cut back length) should be =     R /  Tan(deg/2) = 162/Tan(22.5) = 391 mm
 SCB(short cut back length) should be=    R X Tan(deg/2) =  162 X Tan(22.5)=67 mm

But in shop actual dimensions are LCB =    378 mm
      SCB=     40 mm

Please give solution ... 

how to make template please advice me   

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...