Sunday, February 4, 2018

[MW:27310] regarding precautions to be taken while conducting PQR

Dear sirs,

We are going to conduct PQR for 3" x 5.49 mm with root ER 80S Ni1(Process - GTAW), fillup & final with E 7018 C3L (Process - SMAW) for LTCS pipe in our ongoing project. In the same project other company conduct same PQR but failed in impact test. As impact test conducted at -50 deg., Celsius.

What are the precautions to be taken to conduct PQR without fail in impact test. As we purchased our electrodes which already impact test qualified at -50  deg., Celsius. 

Appreciate your valuable suggestions.

thanks in advance  

N.Kiran kumar,
+91- 7016029043

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...