328.5 Welding Requirements
328.5.1 General (c) Tack welds at the root of the joint shall be made with filler metal equivalent to that used in the root pass. Tack welds shall be made by a qualified welder or welding operator. Tack welds shall be fused with the root
pass weld, except that those that have cracked shall be removed. Bridge tacks (above the weld) shall be removed.
 
Atentamente
Agustin Jimenéz 
+58 4167801321



De: Karunakaran Pasupalagovindasamy <pgkaruna@doosan.com>
Para: ΓΙΩΡΓΟΣ <dilintas@gmail.com>; materials-welding <materials-welding@googlegroups.com>
Enviado: Domingo, 25 de junio, 2017 0:32:36
Asunto: Re: [MW:26647] ASME Tack welder Qualification

Thanks.
How to qualify a person to carry out only tack welding.
Regards,
Karunakaran
On Jun 25, 2017 8:41 AM, "ΓΙΩΡΓΟΣ GEORGIOS D." <dilintas@gmail.com
There is no specific tack welders qualification. If tack welds are performed by non qualified welders they have to be grinded off



Sent from my Samsung Galaxy smartphone.

-------- Original message --------
From: Karunakaran Pasupalagovindasamy <pgkaruna@doosan.com>
Date: 23/06/2017 13:26 (GMT+02:00)
To: materials-welding@googlegroups.com
Subject: [MW:26639] ASME Tack welder Qualification

Dear Experts,
Is there any ASME clause for Tack welder qualification?
Kindly share the input.
 
Regards,
Karunakaran. P.G.
 
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...