Sunday, June 25, 2017

Re: [MW:26648] ASME Tack welder Qualification

The tack welder clause available in AWS D1.1 with hammer break test with shown complete fusion .

Thanking You,

With Regards..
Dinesh V Somwanshi
Api 570, Cswip 3.1,Bgas 2
Authorised Certified Piping, Welding, Painting Inspector.
00919881344135

On Jun 25, 2017 12:11 PM, "ΓΙΩΡΓΟΣ GEORGIOS D." <dilintas@gmail.com> wrote:
There is no specific tack welders qualification. If tack welds are performed by non qualified welders they have to be grinded off



Sent from my Samsung Galaxy smartphone.

-------- Original message --------
From: Karunakaran Pasupalagovindasamy <pgkaruna@doosan.com>
Date: 23/06/2017 13:26 (GMT+02:00)
Subject: [MW:26639] ASME Tack welder Qualification

Dear Experts,

Is there any ASME clause for Tack welder qualification?

Kindly share the input.

 

Regards,

Karunakaran. P.G.

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...