Saturday, June 24, 2017

Re: [MW:26644] PMI for ER-80s-N1

This is contractual requirements. You need to check your project specifications.
I understand your concern, LTCS does not require PMI, but you have 1% Nickel in filler metal, some cross checks are required, discuss with your client. 
If you use it only for root, any way you can't do PMI on root practically.

On 24 Jun 2017 16:40, "'mervin dio' via Materials & Welding" <materials-welding@googlegroups.com> wrote:
Dear group

Can you please give me a reference if required PMI 
Er-80s-N1. We will used this for LTCS materials.

Regards

Vin

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...