Thursday, June 22, 2017

Re: [MW:26633] E316L16 HOLDING TEMPERATURE

No need. Check with manufacturer recommendation

On 22-Jun-2017 3:57 PM, "Kandula Raju" <rgkandula@gmail.com> wrote:
Boxbe This message is eligible for Automatic Cleanup! (rgkandula@gmail.com) Add cleanup rule | More info

Dear Eperts,

  We have E316L-16 electrode supplied in Vacum pack, can any body suggest what is holding time and temperature while in use under normal temperature and humidity

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...