Re: [MW:26598] Shell plate distortion API 650

Dear sir,
What is shell thkness?

This is the common problem aries in shell buckling.

Stich welding and controlling in fillet size, slow welding( with intermittent cooling), to provide the proper stiffner inside and outside will help in avoiding distortion.

Regards
Prasad

--