Hi!Yes weld metal does not come under preview of Qw 407.4 but there is restriction on base metal thk which is 1.1 time T of test plate of PQR so indirectly autometicaly.applies to weld metalIncase of multiprocess PQR.undergoes NR and if the weld thk of each process is more than 19mm in such case each process weld thk qualifies to max thk equal to 1.1T of PQR test plate and for weld less than 19mm it qualifies 2t of each processRegardsHegde Prakash--
On Sun, 4 Jun 2017 at 10:42, MW<raghurambathula@gmail.com> wrote:even some time interpretation needs interpretation??
in my opinion, QW 407.4 does not apply to weld metal thickness.
On Saturday, 3 June 2017 09:25:35 UTC+4, vijay Katkar wrote:
Dear Sir,
Need your help on following issue,
I have PQR with 88 mm thickness ( SMAW – 32 mm & SAW -56 mm)and it has normalizing + stress reliving heat treatment. Generally it is used for dish end long seam (where fiber elongation is more than 5%).
As per QW 407.4 Base material thickness T will be qualified 1.1 times of test coupon thickness, in my case it will be 96 mm maximum and deposition thickness will be as per QW 451 table but shall not be more than base metal thickness. As per my assumption SMAW- up to 96mm & SAW- up to 96mm will qualify.
As per interpretation IX 83-102. Both thickness will qualify 1.1 times. It means that SMAW will qualify up to 35 mm & SAW - 61 mm. Is this interpretation valid as per latest code requirement?
I have attached interpretation copy for your reference.
Vijay Katkar
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com .
Visit this group at https://groups.google.com/group/materials-welding .
For more options, visit https://groups.google.com/d/optout .
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com .
Visit this group at https://groups.google.com/group/materials-welding .
For more options, visit https://groups.google.com/d/optout .
Sunday, June 4, 2017
Re: [MW:26581] Re: QW 407.4 Clause requirement
Dear Prakash Sir,
But this interpretation says both the thickness.
I agree with you that T (Base Metal) restriction has been given in QW 407.4 but this interpretation gives different meaning.
Thank you
Vijay Katkar
On 4 Jun 2017 9:32 a.m., "'Prakash Hegde' via Materials & Welding" <materials-welding@googlegroups.com> wrote:
Subscribe to:
Post Comments (Atom)
Re: [MW:35686] HDPE WPS
Refer ASME SEC IX There is separate chapter for Plastic welding . Based on that you have to prepare Sent from my iPhone On 21 Jun 2025, at...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-