[MW:26588] QW 410.10 Use of Multi-Electrode to Single Electrode

Dear All,          

 

Need your help.

 

I have SAW process PQR with three wire combination, Can I use this PQR with single wire ?

 

Equipment is not required Impact test.

 

Change from Single to multi electrode and vice versa  is a supplementary essential variable.

Current & Polarity of these wires are DCEP.


Is there any other variable which restrict to use multi-electrode to single?  please guide me on this.

 

Regards 


Vijay Katkar 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...