Friday, June 2, 2017

[MW:26571] RE: 26568] Re: P1-P1 qualified WPS for welding API 5L PSL2

Dear Sir ,

 

API 5L Gr –B ,  for root pass E 6010 and fill up  and capping pass  E 7018 /

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of jiju balan
Sent: Thursday, June 01, 2017 11:48 AM
To: Materials & Welding
Cc: wiqw@rediffmail.com
Subject: [MW:26568] Re: P1-P1 qualified WPS for welding API 5L PSL2

 

dear team,
what electrode should be used to weld  API 5L GR-B PSL1 pipes.

regards

On Wednesday, January 2, 2013 at 5:32:43 PM UTC+5:30, krishna wrote:

Dear Team,

We have WPS/PQR for SA106 Gr.B(P1-P1) whether this shall be used for welding of API 5L PSL2
seamless & welded pipes for production and welder qualification.

pls share your experiences.

thanks,
krishna

 

Catch India as it happens with the Rediff News App. To download it for FREE, click here

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...