Wednesday, April 5, 2017

Re: [MW:26365] Regarding Heat treatment and post heating.

Normalizing is usually done at 900degC with subsequent cooling on still air

2017-03-31 9:10 GMT+03:00 Mohit Aggarwal <aggarwalmohit05@gmail.com>:
Dear Experts,

We have straighten the pipe material SA234 WP9, PNo. P5B, for qualification of procedure.Now we will have to done Normalizing and tempering of plate welded material.

Kindly suggest at what temperature we should done the Normalizing 

Also let me.konw is there any post heating requirements are there for this material.or not.

Material is SA234WP9 20mm thk drawn  from.pipe into plate hardness is 190 BHN after straightening and cutting processes.

Best Regards,
Mohit Aggarwal.
9821958461

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALTezPOyDC%3Dcwyv9GWzU_VrZMA9vj_nKKSA1un_V1ws9nBhKPQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40B0R6B2v%2B9r0ipELmOBV3_sSqGaRpTyYcEPBqpf0bYXgA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...