Dear ganeshan,
First of all, I want make clear that,
ASME sec Viii for pressure vessel code.
Asme sec ix for welding and brazing related. (Means it is reference code).
And aws d1.1 for structural steel.
Now,
1) Silo and chimney will come into structural part, so pls refer awsD1.1 for any welding and Ndt requirements.
2) Tanks for oil and water services, will comes under API 650.
Pls refer these respective code for Ndt requirements. Also requesting to refer the client specification, for any Ndt requirements.
Pls revert if any query.
Regards
Prasad
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/5b5de534-0765-4889-b556-4ca3a90c8af3%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
Subscribe to:
Post Comments (Atom)
Re: [MW:35289] Welding consumable for S355J2WP material
S355 J2 WP is a weathering structural steel It has better atmospheric corrosion resistance. Use E 8018 - W1/W2 Electrodes This is regular...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-