Hi
Contact your local supplier or nearest ESAB country office.
Regards
P Govindan
On Apr 2, 2017 10:16, "James Maingi" <maingijames99@gmail.com> wrote:
-- Hi--I trust all well,can you assist on the ESAB welding rods certificates1. Item No. 4800324200Lot. SFP162142. Item No. 4800253200Lot No. SFP10186RegardsMaingi
On Wednesday, 19 January 2011 11:13:11 UTC+3, sam bhal wrote:Hi There
Give me the lot no and batch no of the Esab Product.. I shall send it across to you..
Regards
Sameer Bhalla
Fabricast FZC
Dubai
Date: Mon, 17 Jan 2011 08:35:51 +0000
To: material...@googlegroups.com
Subject: Re: Re: [MW:9261] Test Certificate - ESAB
From: muthu_...@rediffmail.com
for getting BTC you have to give the details as asked. then u can able
to get BTC This foolproof is there otherwise without purchasing anybody
will take printout and do false certification
On Mon, 17 Jan 2011 11:48:50 +0530 wrote
>
Hi
If you know the Lot number or batch no , it is easy to get
the BTC .
Or if you know the date of mfg & Plant , you have to
contact Factory manager of Plant to get the BTC
Thanks & Regards,
K. Babu
>----- Original Message -----
From:
Nagarajan
Muthukumarasamy
To: material...@googlegroups.com
Sent: Saturday, January 15, 2011 12:41
PM
Subject: [MW:9223] Test Certificate -
ESAB
>
DEAR ALL
CAN ANYBODY GUIDE METO GET THE TEST CERTIFICATE FROM INTERNET FOR
THE PARTICULAR LOT NUMBERS
BECAUSE
IN LINCOLN IT IS POSSIBLE TO DOWNLOAD FROM THEIR SITE BUT I CANNOT
FIND
ANY EASYOPTION FOR ESAB
FOR ESAB:
THEY ARE ASKING LOT NUMBER AND INVOICE NUMBER
OTHER THAN THIS IF IS IT POSSIBLE MEANS
PLEASE GUIDE ME TO GET IT.
>--
>
>
>Nagarajan.M
>00967 713800656
>
>
--
>To post to this group, send email to
material...@googlegroups.com
>To unsubscribe from this group, send
email to materials-weld...@googlegroups.com
>For more options,
visit this group's bolg at http://materials-welding.blogspot.com/
>The
views expressed/exchnaged in this group are members personel views
and meant
for educational purposes only, Users must take their own decisions
w.r.t.
applicable code/standard/contract documents.
>
--
>
To post to this group, send email to material...@googlegroups.com
>
To unsubscribe from this group, send email to materials-
welding+u...@googlegroups.com
>
For more options, visit this group's bolg at http://materials-
welding.blogspot.com/
>
The views expressed/exchnaged in this group are members personel views
and meant for educational purposes only, Users must take their own
decisions w.r.t. applicable code/standard/contract documents.
>
Dear Sir,
Thanking You,
Honesty is the best Policy
With Warm Regards,
Muthu Barathi P
Mobile No:00962788269821 (Jordan)
00962775401951
--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
http://www.linkedin.com/groups/MaterialsWelding- 122787?home=&gid=122787&trk= anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com .
To post to this group, send email to materials-welding@googlegroups.com .
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/ .0de95d4c-9f9b-4fdc-888e- aa012ab8d015%40googlegroups. com
For more options, visit https://groups.google.com/d/optout .
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANiuf9cfZP-VYGYjx7Ce-8-zUS309zA-F%3D_sLY9h-sfU-92uSg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
No comments:
Post a Comment