Re: [MW:25867] Piping alignement tolerance as per ASME B31.1

ISO 13920



Sent from my Samsung Galaxy smartphone.

-------- Original message --------
From: raneesh pk <pkraneesh@gmail.com>
Date: 02/01/2017 11:23 (GMT+02:00)
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: Re: [MW:25863] Piping alignement tolerance as per ASME B31.1

Thank you for your reply.
Referring  fig 127. 3 in B31-1, give tolerance of weld joint prior to fit-up.I am asking tolerance of pipe straightness/ verticality and elevation while installing pre-assembled pipe spools

On Thursday, December 29, 2016 at 7:02:50 AM UTC+4, George Dilintas wrote:
see fig 127. 3 in B31-1

2016-12-27 10:52 GMT+02:00 Raneesh.PK <pkra...@gmail.com>:

Dear Experts,

Construction code - ASME B.31.1 (Fuel gas system)

Service - Fuel gas system

I wanted to know how much tolerance can accept  while doing piping alignment inspection like straightness checking , elevation checking dimensional checking etc

Nothing was mentioned in contract documents and project specification.

Please provide the reference.



*RANEESH.PK 

*QA/QC-WELDING*




--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGRQ%2BmV1fhOaGx1CuBcEUxVLs3WkGNoj_OgBuO9fsmMdu8V6dA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/5a2a4193-2060-4d6f-8930-da7157e4c303%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...