Re: [MW:25776] reg: Maximum interpass temperature in a WPS

Hi Prince,
As Interpass temperature is essential variable for your Client; then keep your interpass temperature as 68 + 55°C ie 123°C as addressed in ASME Sec IX.

Aly

On Mon, Nov 28, 2016 at 9:17 PM, Prince C thomas <princecthomas@gmail.com> wrote:
Dear Sir's,

Kindly reply to  my below query:

We have project approved WPS with following details:

Material Spec: ASTM A106 Gr.B

P no:1/Group no:1

Material thickness: 1.5 -14.22 mm

Welding process: GTAW+SMAW

GTAW-Filler wire : ER 70S-2

SMAW-Electrode: E 7018

Preheat - 10 deg minimum

Interpass temp: 200 Deg C Maximum

In the PQR: pre heat temperature:38 deg C

                  Interpass temperature: 68 deg C maximum



Since interpass temperature is not a essential variable (Impact test is not applicable); but still our client is asking to recheck the max.interpass temperature value ( 200 Deg C) in the WPS. How to convince client to get approval on the same?






--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/cb942dff-ef50-4ad8-bd7c-a62ed99ac06b%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOenW4hh7wFSy3ke5wLnJKTEcF9wxxB53utMJM2a%3DNTezz8JSQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...