Tuesday, November 29, 2016

Re: [MW:25773] reg: Maximum interpass temperature in a WPS

Sir
If client spec addresses the IP temp restriction we have to follow the same Generaly.some of the clients are particular about IP.Heat input as.it controls the properties of weld.Haz Therefore it is better to follow to avoid any any further argument with client 
Hegde


On Mon, 28 Nov, 2016 at 22:47, Prince C thomas
<princecthomas@gmail.com> wrote:
Dear Sir's,

Kindly reply to  my below query:

We have project approved WPS with following details:

Material Spec: ASTM A106 Gr.B

P no:1/Group no:1

Material thickness: 1.5 -14.22 mm

Welding process: GTAW+SMAW

GTAW-Filler wire : ER 70S-2

SMAW-Electrode: E 7018

Preheat - 10 deg minimum

Interpass temp: 200 Deg C Maximum

In the PQR: pre heat temperature:38 deg C

                  Interpass temperature: 68 deg C maximum



Since interpass temperature is not a essential variable (Impact test is not applicable); but still our client is asking to recheck the max.interpass temperature value ( 200 Deg C) in the WPS. How to convince client to get approval on the same?






--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/cb942dff-ef50-4ad8-bd7c-a62ed99ac06b%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/296923631.2378648.1480388666548%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...