Tuesday, November 22, 2016

Re: [MW:25750] Difference Between Carbon Steel and Wrought Carbon Steel

Wrought means simply worked, accordingly all items fabricated subject to rolling, forging, extrusion, etc are wrought 
I.e all items except casting are wrought 

A.eissa


On Fri, 18 Nov, 2016 at 7:04 am, Vinod Palande
<palande.v85@gmail.com> wrote:
Dear Experts,

In project specification mentioned as Wrought products shall be free from elongated inclusions.

A. Which product to be considered as wrought product. (i.e Seamless Pipe or Fittings or Both)


In ASME Sec II SA 106 pipe described as carbon steel and SA 234 fittings described as wrought carbon steel.

B. What is difference between carbon steel and wrought carbon steel.

Thanks in Advance.

Regards,
Vinod V. Palande.



--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/16e04d6b-05a9-49d9-b663-fd189424bd78%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1590271965.1471194.1479758469397%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...