For offshore structural members as per EEMUA 158

7.2.2    Timing of Final Inspection and NDT

All visual inspection of completed welds shall be carried out as soon as is practical after the item has cooled down to ambient temperature .

NDT shall not be carried out until at least 48 hours have elapsed following completion of welding. However, for welds/items which are subject to a PWHT requirement , the specified inspection and NDT may be performed and reported immediately following completion of the PWHT process. but not before the welds/items have cooled to ambient temperature.


Regards

Kingsly Geo

BUREAU VERITAS - Abu Dhabi


On 1 October 2016 at 10:48, Saulo MU <pablo.cartagena.androide@gmail.com> wrote:
As mhs indicates ,the need of inmediate inspección vía UT/RT is to control the welder performance.
So stop welders with a % of defects found .Lets say 5% ( percentage agreed).Also in case of failure you must duplicate quantity of tests.Till this reduces or to give permanent vacations (on the contrary) to this welder.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/2e2163e9-9c8c-4f5d-8d7d-6dab6d473978%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAAR7VZ8hf2zJXhhkV_hQXu7FSJ8p0HB6QuEtWk_zinHkaPAVxg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...