Re: [MW:25745] MPI on painted joint

If you follow by the letter ASME V and you can demonstrate performance as per Asme V requirements  then you can use it on painted surface under the same conditions.
However it is not advisable 




Sent from my Samsung Galaxy smartphone.

-------- Original message --------
From: george keribo <berepele@gmail.com>
Date: 18/11/2016 14:47 (GMT+02:00)
To: materials-welding@googlegroups.com
Subject: [MW:25727] MPI on painted joint

Please I wanted to know any code reference for painted surface magnetic particle test

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAF27W4Ss47uNCqgDQUGh0%2BpLM40NH8wqJiP4aaDsWxio_mWqHQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...