Sunday, November 20, 2016

Re: [MW:25745] How to do testing of Reinforced pad

Leak test by blowing into the vent hole. For leak test see Asme V



Sent from my Samsung Galaxy smartphone.

-------- Original message --------
From: vinay yadav <yadav.vinayp@gmail.com>
Date: 18/11/2016 09:05 (GMT+02:00)
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:25729] How to do testing of Reinforced pad

Dear Sir,

How to do testing of Reinforced Pad. ?

Best Regards,
Vinay.




--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/8c67ff34-3368-4e41-9b4a-e57167496087%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...