Re: [MW:25744] RE: 25727] MPI on painted joint

Alan thanks
But I think it's possible cause we have magnetic test method to detect paint coating thickness so it's possible to carry out MPI on a painted joint. I really want to know if there is a code reference or a publication that might say something like that.  Thanks for your contribution I do appreciate.


On Nov 19, 2016 14:02, "Alan Denney" <alan@denney1.freeserve.co.uk> wrote:

My experience is that it does not work,  and this is not surprising. I have had eddy current testing used over painted surfaces to detect underlying cracks with good results, in that cracks were reliably detected. You would need to trial it with coatings on the calibration block.

 

Alan Denney

AKD Materials Consulting Ltd

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of george keribo
Sent: 18 November 2016 12:48
To: materials-welding@googlegroups.com
Subject: [MW:25727] MPI on painted joint

 

Please I wanted to know any code reference for painted surface magnetic particle test

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAF27W4Ss47uNCqgDQUGh0%2BpLM40NH8wqJiP4aaDsWxio_mWqHQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.


This email has been scanned by BullGuard antivirus protection.
For more info visit www.bullguard.com

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/000201d24260%242abba580%248032f080%24%40denney1.freeserve.co.uk.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAF27W4QA9H9Ga6vXJZ15MosQ%2BGhFa9KOn31dXrj_GvFHVX37vg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...