Re: [MW:25736] How to do testing of Reinforced pad

Dear Mr. Vinay,

In API  650 standard  article 7.3.4  it is recommending  for pneumatic pressure test at 100 KPa (1.05 Bar).Once pressure is applied thru tell tale hole, soap solution shall be sprayed to find any leakage.


Best Regards,

JIJILAL K.M. 
QA/QC Manager,
Thai Jurong Engineering Ltd,
KCE SPP Project,Thailand



On 18 November 2016 at 14:05, vinay yadav <yadav.vinayp@gmail.com> wrote:
Dear Sir,

How to do testing of Reinforced Pad. ?

Best Regards,
Vinay.




--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/8c67ff34-3368-4e41-9b4a-e57167496087%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHmEnHh%3DY3uPJse7zbOGa1k91ZUhgYGgVJ5cx6ct6MDs2_VW9w%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...