Re: [MW:25723] Why xray are use for lower thickness

Dear Sir's,

I agree that , we get better quality of radiograph in xray.
I only want to discussed that,
1) If we want to talk about radiography quality, then if required IQI is visible, then we can say that minimum defects is visible as required IQI is visible.
Code also says that radiographs quality or acceptance, depends on visibility of require IQI.
2) my another point is that, in which section or code, it is mention, that below particular thickness of material, xray to be use and above that thickness, gamma is allowed. So that we can insist contractor to do the same.

Thanks for response.
Expecting the same.

Regards
Prasad

On Nov 16, 2016 17:39, "Kannayeram Gnanapandithan" <kgpandithan@gmail.com> wrote:
no, X-ray is the best one

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349

On Wed, Nov 16, 2016 at 11:48 AM, Prasad Rode <purode333@gmail.com> wrote:
Boxbe This message is eligible for Automatic Cleanup! (purode333@gmail.com) Add cleanup rule | More info

Dear prem and George sir,

Thanks for reply.
I want to ask that if I use the high sourse ir192 and increase the exposure time i.e. time as required by calculation, can I get the good radiographs and using iqi of din standard.
Our thickness of pipe is below 4mm.
We required genuine and technical reason to insist to contractor.
Requesting for response.

Regards
Prasad

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/146532af-75e9-4a75-bde1-3bbf68a60302%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to a topic in the Google Groups "Materials & Welding" group.
To unsubscribe from this topic, visit https://groups.google.com/d/topic/materials-welding/i3qxdjlk_nU/unsubscribe.
To unsubscribe from this group and all its topics, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eOTxmVo1iRL3JV-HpjoAQhY4Jmzg%2BpF8zG7T%3DamsO3ViQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2Bk3Rc_TTUd6cT7L2_f9kKTt8km_1Ezsyp51MA%3DwSd0CJoMwBA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...