[MW:25737] Re: WPS as per ASME SEc. IX

if this WPS will be applied for oil and gas service, you can refer to API RP 582 table A, and ASME IIC for selection wleding consumable

Regards
Kurniatullah Sirajudin

On Saturday, November 19, 2016 at 9:59:26 AM UTC+7, John Manoj wrote:
Dear Experts,

We have the following WPS as per ASME Sec. IX

Base metal - P5B + P8  (6" Sch 40 Pipe)
Welding process -  GTAW
Filler metal -  ER NiCr-3
Preheat temp - 180 degree C
PWHT - Nil
Trailing & backing gas -  Yes (Argon)

Can i use the above procedure for welding of ;

P5B group material fillet welding (seal welding of threaded joints) with ER NiCr-3 or ER NICrMo-3 GTAW process without PWHT 
Hardness test required for HAZ 235HV10.

your expert advice highly appreciated.

Thanks & Regards,
Manoj.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/4097c5df-00dd-447f-b54b-f6fa28a71f4b%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...