Re: [MW:25481] Impact Test

Dear
go for new impact test at -198.

Regards
a p gupta


On Mon, 3 Oct, 2016 at 18:30, Mohd Azam
<azam1976@gmail.com> wrote:

Dear All,

 

Material:                        SS304l ( 5 mm Thick Pipe ASTM A312 TP304L)

Code:                           ASME B31.3

Design Temperature:     -198 Deg C

Welding process:          GTAW

 

 

The available WPS/PQR tested  @ -196 Deg C with GTAW Process in accordance with ASME SEC IX and ASME B31.3 but design temperature -198 Deg C as above indicated material, Can we use available procedure to weld above material.

 

Thanks & Regards,

Mohd. Azam

Doha - Qatar

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABD%2BRXTyf0JYdZ8LtqU4OxQ0zc4oDjMMh1scwyE4pEM6rOJoaw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1281996148.8070620.1475582048276%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35346] Cast-iron welding

Any advice for cast iron welding Sent from Yahoo Mail for iPhone