Tuesday, October 4, 2016

Re: [MW:25478] Cellulose electrode redrying

because it has got more Hydrogen around 30 to 60ppm, if u do baking , H2 will get lost and purpose is defeated


THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349

On Mon, Oct 3, 2016 at 11:43 AM, Pravin G <htcispravin@gmail.com> wrote:
Boxbe This message is eligible for Automatic Cleanup! (htcispravin@gmail.com) Add cleanup rule | More info

Dear expert,

Can anyone advice why cellulose electrode don't need redrying? Any particular Technica reason?

Pravin Poornachandran

Sent from my iPhone

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/672D2E56-43BC-4AE9-8B4B-ED48562CB124%40gmail.com.
For more options, visit https://groups.google.com/d/optout.


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eOAv0ZKuni5J4uBFw7z4A6cNBF0uj_eU0tHdVbdvMmRDA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35346] Cast-iron welding

Any advice for cast iron welding Sent from Yahoo Mail for iPhone