[MW:25474] Qualification of S.S. wire/flux combination

Dear experts,

As we know, there are some standards for qualification of C.S. wire/flux combination such as AWS A5.17 which describe the method for welding a test plate (test plate material / schematic of test assembly / welding parameters) and also testing of such a test plate (NDT / Chemical / Mechanical).

Could you reference similar standard for qualification of S.S. wire/flux combination? I couldn't find it in AWS or ISO.

Regards

--
M. Shokri Arfaei
ASNT NDT Level III
International Welding Engineer

Mob.:+98 912 1394023




--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAC8uMtuPCY8gnkicZ4DB%3Dsn8qpe53XfwNOZ85ctfCXTO5CpwXA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...