Thursday, August 4, 2016

Re: [MW:25194] P number grouping for IS 2062 material

Could anyone provide thermal conductivity of IS2062 material for various temperatures?

On Friday, 23 September 2011 16:10:03 UTC+5:30, Bathula Raghuram (Mumbai - PIPING) wrote:

IS2062 has been included in ASME BPV Sec IX 2011 addenda under P number 1 Group number 1 for all the three grades (i.e. A,B,C)

 

 

 

 

From: material...@googlegroups.com [mailto:material...@googlegroups.com] On Behalf Of Bathula Raghuram (Mumbai - PIPING)
Sent: Monday, January 31, 2011 9:12 AM
To: 'material...@googlegroups.com'
Subject: RE: [MW:9569] P1 no Range

 

IS 2062 is an unlisted material

SS 410 will under P number 6 ( refer table QW/QB 422)

 

From: material...@googlegroups.com [mailto:material...@googlegroups.com] On Behalf Of puneet takiar
Sent: Sunday, January 30, 2011 8:04 PM
To: material...@googlegroups.com
Subject: Re: [MW:9565] P1 no Range

 

Hello!

Can anybody tell me in which P. no IS 2062 grade A and SS 410 will fall and how to search in ASME sex IX table.

Regards, 



--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/ef910007-c378-4036-81d1-e8568d523ddf%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...