Dear Mr. Shah,

First you have to purchase electrodes as per the your specified requirment.

In addition to the above, for achieving this you have to take care for following:

1. No filing/ brushing/ grinding etc. should be done on welds before measuring ferrite %
2. Allow weld to cool in open air
3. The ferrite should be measured immediately after cooling of the welds

Best Regards,
Rajnish


--------------------------------------------
On Fri, 5/20/16, SATISH SHAH <sbdr1912@gmail.com> wrote:

Subject: [MW:24816] Ferrite % 4-8 of E309LMo
To: "Materials & Welding" <materials-welding@googlegroups.com>
Date: Friday, May 20, 2016, 3:49 PM

Dear Expert,

Let me know Ferrite 4 - 8 % is possible to obtain of
Electrode 309LMo as weld condition.


Regards

SATISH SHAH




--

http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members
personel views and meant for educational purposes only,
Users must take their own decisions w.r.t. applicable
code/standard/contract documents.

---

You received this message because you are subscribed to the
Google Groups "Materials & Welding" group.

To unsubscribe from this group and stop receiving emails
from it, send an email to materials-welding+unsubscribe@googlegroups.com.

To post to this group, send email to materials-welding@googlegroups.com.

To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/8c7f5e73-c5e0-4c60-ab4f-92cb2537713b%40googlegroups.com.

For more options, visit https://groups.google.com/d/optout.


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1960327134.1201241.1466430002179.JavaMail.yahoo%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...