Re: [MW:25019] Relation between diffusible hydrogen and welding current

Research papers demonstrate the contrary

Sent from my BlackBerry 10 smartphone.
From: 'prem_nautiyal26' via Materials & Welding
Sent: Τρίτη, 28 Ιουνίου 2016 - 09:12
To: materials-welding@googlegroups.com
Reply To: materials-welding@googlegroups.com
Subject: Re: [MW:25017] Relation between diffusible hydrogen and welding current


There is no relation between diffusible hydrogen content and Welding current.



Sent from my Samsung Galaxy smartphone.

-------- Original message --------
From: Pravin G <htcispravin@gmail.com>
Date: 27/06/2016 16:00 (GMT+05:30)
To: 'Agustin Jimenez' via Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:25011] Relation between diffusible hydrogen and welding current

Dear expert,

What is the correlation between diffusible hydrogen and welding current.

How does Welding current affects diffusible hydrogen ? Based on any specific code or theory?

Kindly help to explain.

Pravin Poornachandran
Singapore
Sent from my iPhone

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/5DFF92D3-8F9F-4BA9-A964-E41BEB02E7CA%40gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/v8q94dia7bqepf9lwwlby3f4.1467039768760%40email.android.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...