Monday, June 20, 2016

Re: [MW:24976] pre heat inconel-625

Its not preheating.Its baking.Its required.Follow as per manufacturer guidelines.

Regards,


 Muniyandi Chithiran MBA.,MIIF,
AWS Certified Welding Inspector,
ISO 9001,14001,17025, Lead Auditor,
NDT Level II-RT,UT,MT,PT,

Mobile: 0091 95855 40965,99947 65591

Go where you are celebrated not where you are tolerated.
Comfort is the enemy of achievement.

On Sat, Jun 18, 2016 at 6:50 PM, Ali Zarasvandi <ali.zarasvandi@gmail.com> wrote:
hi

do we need preheat of electrode when using inconel-625









--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/e9e2daff-7d56-4611-aa40-97edced03eef%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMJSSYk1WW%3DE%3DJ8teKioUXmzL3DE8rDSKe91Nxgn0VFUvpcXdg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...