Re: [MW:25006] COMBINATION PROCESS WPS

Dear Balaji
Yes you can use same PQR,but revise the WPS 
Note: Only change non essential parameter

Regards 
M.Sajid.

On Sat, Jun 25, 2016 at 1:31 AM, balaji srinivasan <bolukbalaji@gmail.com> wrote:

Dear all,

We have WPS-A for stainless P8 to 08  witith Gtaw+ smaw thickness limit is gtaw 8mm and smaw 14mm.
Now our construction team is trying to weld only gtaw process for upto 8mm weld joints with same WPS -A .
Is it possible to use it or I want make new WPS for gtaw with supporting of same PQR.
Please advice.

Regards,
Balaji.M

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAK1csg3c12yx1TKv2e017UVobthBT5YWAkD9UMGjC2ricpWbHA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAAKkJLc0Ss30QFargSACf5Ag85MoW3yz8M9oGq_7VGfn6q4vAw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...