[MW:24993] Re: Fracture test

Hi,


Please refer below image from ASME sec IX (QW462.4(c)) for fillet weld performance qualification.

As per drawing, cut the coupon and apply force.


  
  

Note: Also, you should carry out Macro test in order to qualify the welder (QW452.5).

  
  



Thank you.

Regards,
Dhanasekaran S,

Aker Solutions.

Mob: +91 75079 17709  I   +91 70401 02428 



On Wednesday, 22 June 2016 07:55:43 UTC+5:30, MAGHROUD Moussa wrote:

Dear expert.
I have to performe fracture test to qualify welders. The coupon is made by pipe 4"  to plate position 5F. My question is how to execute it?

Best regard


Envoyé depuis un mobile Samsung

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c73ecd9a-9f32-4a37-bf16-9fd888253ab6%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...