Dear Mac,

The chemical composition/properties of the tested material are aprx. meeting with SA335 P1/P2.

It should be tested when the material was received through PMI to confirm major elements like Cr, Mo, etc.

Regards,
Rajnish

--------------------------------------------
On Wed, 6/29/16, 'Mac Palola' via Materials & Welding <materials-welding@googlegroups.com> wrote:

Subject: [MW:25021] Chemical Composition
To: "Materials & Welding" <materials-welding@googlegroups.com>
Date: Wednesday, June 29, 2016, 12:07 AM

Dear Sirs,

Project: Coal fired power plant ASME B31.1 CODE

We received a pipe material 1 inch dia with a material of
A335 P91.
This material had been welded.
During operational, 2 years after, one pipe burst out.
We send for testing to check the chemical composition.
Please see attached docs.

I checked on ASME Section II Part A and it was very far from
the chemical requirements of A335 P91.

My query is that, what kind of pipe material base on the
result of test report.

Your reply to this query will be highly appreciated.


Regards,

Mac








--

http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members
personel views and meant for educational purposes only,
Users must take their own decisions w.r.t. applicable
code/standard/contract documents.

---

You received this message because you are subscribed to the
Google Groups "Materials & Welding" group.

To unsubscribe from this group and stop receiving emails
from it, send an email to materials-welding+unsubscribe@googlegroups.com.

To post to this group, send email to materials-welding@googlegroups.com.

To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/5c7fba20-d6e9-4fc8-b7b5-472c4cf79057%40googlegroups.com.

For more options, visit https://groups.google.com/d/optout.


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1647366674.708503.1467175343070.JavaMail.yahoo%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...