Re: [MW:24969] IMPACT TEST REQUIREMENT

P1 G1 to P1 G2 qualifies P1 G1 to P1 G2, P1 G2 to P1 G2 and P1 G1 to P1 G1. Hope your query is addressed.

Sent from my iPhone

On Jun 17, 2016, at 11:37, balaji srinivasan <bolukbalaji@gmail.com> wrote:

Dear All,


As per ASME SEC-IX   change in material Group is Supplementry  essential variable (403.5)

based on above i need your experience  If iam qualified PQR p1 group-1 to p1 group-2 tow different group welded it self so the  qualfied range will be p1 group1 and p1 group 2.

or only this PQR is qualified group 1 to group-2 qualified.

also please advice i need to qualify group 1 separate and group 2 separate PQR.


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAK1csg3Drkobg2%3DG9Lyy0CMd3WbM%2BOq_9e2GkJLoC-QxBUhP0A%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...