Monday, June 20, 2016

Re: [MW:24980] hardox

The only way to drill Hardox is to use the proper tooling,making Hardox soft is defeating the purpose of using this material.
Regards,
Iain.

sarbjeetsingh wrote:

Dear Experts.,

How to make hardox material soft for drilling.
is any othe way to drill hardox with HSS drill

regards
Sarb

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
<http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm>
The views expressed/exchnaged in this group are members personel views
and meant for educational purposes only, Users must take their own
decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google
Groups "Materials &a mp; Welding" group.
To unsubscribe from this group and stop receiving emails from it, send
an email to materials-welding+unsubscribe@googlegroups.com
<mailto:materials-welding+unsubscribe@googlegroups.com>.
To post to this group, send email to
materials-welding@googlegroups.com
<mailto:materials-welding@googlegroups.com>.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/CANLC91EHh09kvsA_LXzeENZ3%2BREGsCRr2X%2B-SXxt8eB_Qw%2BR%2BA%40mail.gmail.com
<https://groups.google.com/d/msgid/materials-welding/CANLC91EHh09kvsA_LXzeENZ3%2BREGsCRr2X%2B-SXxt8eB_Qw%2BR%2BA%40mail.gmail.com?utm_medium=email&utm_source=footer>.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...