Dear Mr.Harshal,

Penetrameter standard - EN-462- availability - Eastwest Engg&Electronics Mumbai. Procedure have to be developed for the specific case of thickness range, EB weld etc.

Regards

Mohan Ananthanarayanan
DGM Quality-External Fabrication
VSSC ISRO



On Wed, 22 Jun 2016 02:29:19 -0700 (PDT), Harshal Waghule wrote
> Dear All
> I am going to qualify welding procedure for tantalum and zirconium.
> if anybody have please send me for reference.
> and i need the RT procedure for zirconium and tantalum, i have searched the penetrameter (IQI) but i could not found in market.
>
> Regards,
> Harshal Waghule
> --
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
> ---
> You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
> To post to this group, send email to materials-welding@googlegroups.com.
> To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/eb3e661f-f1aa-4d70-9f46-694f2aeec181%40googlegroups.com.
> For more options, visit https://groups.google.com/d/optout.


No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...